The products produced could have been more satisfactory since we launched the wet-mixed mortar project last year. The powder additives can’t make the mortar smooth, and it is not easy to dry after being applied to the wall. The inner wall is thinner and not very flaky, and the outer wall is partially peeled off at the back even if done twice, and the previous layer will fall off after the second time, and the mortar used for plastering the inner wall is not smooth.
interior wall
P ·0 42.5 Cement: 200 Mineral powder: 70 River sand: 1350
Additive: 0.6
outer wall
Cement: 220 Mineral powder: 70 River sand: 1350 Additive: 0.7
interior wall
P ·0 42.5 Cement: 200 Mineral powder: 70 River sand: 1350
Additive: 0.6
outer wall
Cement: 220 Mineral powder: 70 River sand: 1350 Additive: 0.7