    The ready-mixed wet-mixed mortar is used for the tensile bonding test, and the mortar on the specimen quickly falls off. What's the matter?

    Whether the bottom plate is made according to the standard, it should use a rough surface and no oil on it.
  2. L

    Mortar admixtures have poor plasticity, which causes mortar hardly maintains its optimum state. Who can give me some directions about this?

    Mortar admixtures have poor plasticity, which causes mortar hardly maintains its optimum state. Who can give me some directions about this? When the machine has just finished mixing, the overall condition of the mortar looks good. After standing for 2 hours, the mortar began to loosen. I...